<p>The oxidation products of electrode pitch (category C) in a reactor with large gas capacity are considered. The influence of the oxidation time on the softening point and yield of volatiles in the production of high-temperature coal tar pitch is determined. In the experiments, the oxidation of electrode pitch is investigated as a function of the oxidation time and the maximum temperature. Oxidation occurs in the range 260–360°C. The air flow rate is 800 L/kg h. The yield of products, the softening point, and the yield of volatiles are determined as a function of the oxidation time. The increase in softening point may be attributed to the increase in oxidation time at temperatures above 300°C. The conditions for the production of high-temperature coal tar pitch by oxidation of electrode pitch are established. The dependence of the carbonizate yield on the oxidation time is determined.</p>

错误:搜索内容不能为空,请输入英文关键词
错误:关键词超出字数限制,请精简
高级检索

Oxidation Products of Electrode Pitch in a Reactor with Large Gas Capacity

  • R. Yu. Kovalev,
  • A. P. Nikitin

摘要

The oxidation products of electrode pitch (category C) in a reactor with large gas capacity are considered. The influence of the oxidation time on the softening point and yield of volatiles in the production of high-temperature coal tar pitch is determined. In the experiments, the oxidation of electrode pitch is investigated as a function of the oxidation time and the maximum temperature. Oxidation occurs in the range 260–360°C. The air flow rate is 800 L/kg h. The yield of products, the softening point, and the yield of volatiles are determined as a function of the oxidation time. The increase in softening point may be attributed to the increase in oxidation time at temperatures above 300°C. The conditions for the production of high-temperature coal tar pitch by oxidation of electrode pitch are established. The dependence of the carbonizate yield on the oxidation time is determined.