<p>We report the green synthesis, structural characterization, optical measurements, and theoretical modeling of ZnSe and ZnSe/ZnS quantum dots (QDs) synthesized via a rapid aqueous method using thioglycolic acid (TGA) as a stabilizer. The synthesis was carried out at 90 °C and pH 8.5, employing zinc acetate, NaHSe as a selenium source, and thiourea for ZnS shell growth. X-ray diffraction (XRD) analysis confirmed cubic-phase ZnSe with a dominant (111) peak, while ZnSe/ZnS core–shell samples exhibited additional peaks attributed to hexagonal ZnS, indicating successful passivation. Williamson–Hall analysis yields a core crystallite size of ~ 2.3 nm and reveals a compressive interfacial strain of − 2.2% in the core–shell heterostructure. Optical characterization via UV-Vis and photoluminescence (PL) spectroscopy techniques showed redshift in both absorption and emission with increasing reaction time and temperature, consistent with quantum size effects and shell-induced modifications. Theoretical modeling by using modified Brus equation based on Kane’s effective mass approximation, and a recently developed thermoelastic strain theory quantitatively explained the bandgap evolution by accounting for size-dependent confinement and elastic strain at the core–shell interface. Calculated bandgap values showed strong agreement with experimental data: 3.67–3.71&#xa0;eV from absorption and 3.39–3.41&#xa0;eV from PL. The integration of green chemistry and strain-sensitive bandgap engineering underscores the potential of the QDs for low-toxicity optoelectronic and biosensing applications.</p>

错误:搜索内容不能为空,请输入英文关键词
错误:关键词超出字数限制,请精简
高级检索

Structural and optical properties of ZnSe and ZnSe/ZnS quantum dots prepared by using green method

  • Imene Belaribi,
  • Mesut Balaban,
  • Soumia Bendella,
  • Hilmi Ünlü

摘要

We report the green synthesis, structural characterization, optical measurements, and theoretical modeling of ZnSe and ZnSe/ZnS quantum dots (QDs) synthesized via a rapid aqueous method using thioglycolic acid (TGA) as a stabilizer. The synthesis was carried out at 90 °C and pH 8.5, employing zinc acetate, NaHSe as a selenium source, and thiourea for ZnS shell growth. X-ray diffraction (XRD) analysis confirmed cubic-phase ZnSe with a dominant (111) peak, while ZnSe/ZnS core–shell samples exhibited additional peaks attributed to hexagonal ZnS, indicating successful passivation. Williamson–Hall analysis yields a core crystallite size of ~ 2.3 nm and reveals a compressive interfacial strain of − 2.2% in the core–shell heterostructure. Optical characterization via UV-Vis and photoluminescence (PL) spectroscopy techniques showed redshift in both absorption and emission with increasing reaction time and temperature, consistent with quantum size effects and shell-induced modifications. Theoretical modeling by using modified Brus equation based on Kane’s effective mass approximation, and a recently developed thermoelastic strain theory quantitatively explained the bandgap evolution by accounting for size-dependent confinement and elastic strain at the core–shell interface. Calculated bandgap values showed strong agreement with experimental data: 3.67–3.71 eV from absorption and 3.39–3.41 eV from PL. The integration of green chemistry and strain-sensitive bandgap engineering underscores the potential of the QDs for low-toxicity optoelectronic and biosensing applications.